Tag
#welding
15 topics across all disciplines.
Refractory anchoring — holding a ceramic lining onto a steel wall
Why a lining needs anchors at all, the V, Y, hexmetal and ceramic arrangements and where each belongs, why anchor tips are coated before the refractory goes on, and why an anchor is the part of the system most likely to decide when the lining fails.
Welding processes, WPS and NDT — what happens before an arc is struck
SMAW, GTAW, GMAW and the rest, explained by what they are good at. Then the paperwork that makes a weld legal — WPS, PQR and welder qualification — and how welds are inspected.
Material degradation — sensitisation, hardness limits and galvanic attack
Why welding can ruin the corrosion resistance of stainless steel without touching the weld, what the three conditions for galvanic corrosion are and which one to break, why sour service controls hardness rather than strength, what carbon equivalent predicts, and why zinc and stainless are kept apart.
Non-destructive examination — choosing the method and reading the result
Why every NDE method is blind to something, what magnetic particle cannot do on stainless, why ultrasonics can miss a crack lying the wrong way, the difference between an indication and a defect, and why the examiner's qualification is part of the result.
Pipe support standards and details — reading SP-58, SP-69 and a project detail sheet
What the support standards actually fix, why a project standard detail is a specification rather than a catalogue, the welded attachment problem on alloy and sour service, shoes and trunnions and shields, and what goes wrong when a support is left to the field.
Section IX essential variables — what invalidates a procedure qualification
Why a WPS can be revised freely in some respects and requalified from scratch in others. Essential, non-essential and supplementary essential variables, the ranges a PQR actually qualifies, and the low-temperature trap that turns a harmless change into a requalification.
Reading a WPS and a PQR — what is on the sheet and what the tests proved
The practical document skill — what each field on a welding procedure specification is for, what a qualification record actually recorded, and what tensile, bend, impact, macro and hardness results each demonstrate about the joint.
Welder qualification and continuity — the ranges a ticket covers, and the register nobody updates
What a welder performance qualification actually establishes, the ranges it carries in thickness, diameter, position and process, how continuity lapses at six months, and why the expired ticket is always found after the weld is made.
Joint preparation and fit-up — the hold point you only get once
Bevels and root gaps, internal misalignment and the limits on it, why trimming or counterboring is allowed where grinding the bore is not, tack welds as part of the final weld, and what an inspector checks in the minutes before the root goes in.
Preheat and post-weld heat treatment — hydrogen, hardness, and reading the chart
What preheat is actually for, why interpass temperature has a ceiling as well as a floor, when PWHT is required and when it may be exempted, how to read a chart recorder trace against the specified cycle, and the hardness survey that decides it in sour service.
Structural steel connections — bolting, pretension and erection
The difference between a bearing connection and a slip-critical one, what pretension actually does and why it needs hardened washers, how a tension control bolt tells you it is done, why slotted holes exist and what they must not be used for, and what to check before a crane lifts anything.
Steel metallurgy and weldability
What the chemistry on a mill certificate actually controls, why carbon equivalent decides whether a joint needs preheat, what the heat-affected zone is and why its coarse-grained band is the weakest part of a good weld.
Fatigue and fracture in structural steel
Why welded steelwork cracks at loads far below yield, how EN 1993-1-9 detail categories work, what a fatigue fracture face tells an inspector, and how brittle fracture differs from fatigue and why cold weather changes the answer.
Structural NDT and inspection access
How to choose a non-destructive testing method from the flaw you expect rather than from habit, what each method is blind to, and how scaffold, platforms, rope access and drones decide what a structural survey can actually cover.
Steel repair and strengthening
What to do once a defect has been found — how to establish the cause before repairing the symptom, whether old steel can safely be welded at all, the four ways of dealing with a crack, and how to strengthen a member so the fix matches the way it was actually failing.